Guangzhou, Guangdong, China.

Hot Gas Filtration with Ceramic Fiber Filter Tubes

Ceramic fiber filter tubes for hot gas filtration
Ceramic fiber filter tubes for hot gas filtration

Anchor-Filter supplies rigid ceramic fiber filter tubes and complete hot gas filtration units that clean industrial exhaust at temperatures where bag filters and ESPs reach their limits. One vessel removes dust, acid gases, NOx and dioxins: particulate emissions stay below 5 mg/Nm³, DeNOx efficiency exceeds 95% inside the SCR window, and filter grades cover continuous service at 600 °C and 1,000 °C.

Request a QuoteSee How It Works

Why Conventional Filters Struggle with Hot Gas

Plants running glass furnaces, incinerators, kilns and smelters face the same constraint: the gas that needs cleaning is hot, often corrosive, and carries fine PM2.5 and sub-micron particles. Cooling the gas first wastes recoverable heat and adds equipment. The three mainstream options compare as follows:

TechnologyStrengthsLimits in hot gas service
Electrostatic precipitator (ESP)Good collection efficiency; no secondary pollutionHigh energy consumption; performance swings with fuel and fly ash; large footprint; cannot hold ultra-low emission levels
Bag filter (fabric baghouse)Good filtration; works with alkaline sorbent injection against acid gasesNot heat-resistant; hardens and ruptures in acid gas; short service life; mediocre PM2.5 capture; unstable ultra-low emission
Ceramic fiber filter (CF)Very high filtration capacity; resistant to high temperature, acid and alkali; saves water and energy; long service life; no secondary pollution; stable ultra-low emission—

Ceramic filter tubes are rigid, self-supporting candles mounted on the tubesheet of a pulse-jet collector, exactly where filter bags would sit — which makes them a direct retrofit path for existing baghouses. → How to Retrofit a Baghouse to Ceramic Candle Filters

One Unit, Four Duties: Dust, Acid Gas, NOx, Dioxins

A CF hot gas filtration unit is more than a dust collector. With dry sorbent injection and catalyst-loaded filter tubes, a single vessel handles four pollutant groups:

  • Dust — captured on the rigid tube surface and pulse-cleaned; outlet stays below 1 mg/Nm³, meeting ultra-low emission requirements.
  • Acid gases (SO₂, SO₃, HCl, HF) — neutralized by injected NaHCO₃ or Ca(OH)₂ dry sorbent upstream of the tubes; a dry process that uses no water and creates no wastewater.
  • NOx — removed SCR-style by catalyst loaded inside the tube wall, with ammonia or urea injection. The dust cake stays on the tube surface, so the catalyst is shielded from dust blinding and heavy-metal poisoning.
  • Dioxins and organic HAPs — decomposed inside the tube wall by selective catalytic oxidation (SCO) into CO₂, H₂O and HCl; no activated carbon bed and no other chemical dosing is required for dioxin destruction.

Optimal combined operating window for dust + acid gas + NOx duty: 250–350 °C.

PollutantWorking windowDocumented performance
PM2.5 / PM10 / sub-micron dustup to ~1,050 °C (grade-dependent)Outlet <1 mg/Nm³; running ΔP typically <1,500 Pa, long-term <2,500 Pa
NOx (SCR, NH₃/urea)280–400 °C>95% DeNOx at 280 °C and above; catalyst service life 7–9 years, 5 years guaranteed
SO₂ / SO₃ / HCl / HF (dry sorbent)Na-based sorbent 320–400 °C; Ca-based 300–450 °CNa-based sorbent: 85–95% removal (depends on sorbent dose, gas humidity, process design, operating conditions)
Dioxins / O-HAPs (SCO)170–300 °C, optimum 220–260 °C; inlet SO₂ <50 mg/Nm³Dioxin destruction up to 99.5% TEQ; integrated trains achieve dust ≤5, SO₂ ≤30, NOx ≤50 mg/Nm³ (S.T.P., dry)
Mercury (Hg)Brominated powdered activated carbon 260–430 °C>90% removal (activated carbon at 200 °C: 70–80%)
VOC230–260 °C95% removal
CO200–300 °CRemoved together with NOx duty

Ceramic Filter Tube Specifications (White Tube, Non-Catalyst)

Ceramic filter tubes in protective foam packaging
White ceramic filter tubes in protective packaging, ready for shipment

The workhorse element is a vacuum-formed ceramic fiber tube with a graded pore structure — pore size graduates from the outer surface inward, so dust forms a surface cake while the wall depth stays open.

Elements ship in foam-supported cartons, stackable up to 10 high, and should be unpacked only immediately before installation.

ItemSpecificationNotes
DimensionsØ150 × Ø110 × 3,000 mm20 mm wall
Unit weight7.5 kg (batch tolerance <0.5 kg)White tube
Forming processIntegrated vacuum negative-pressure formingEuropean process
Porosity>83%
Fiber blend70% domestic + 30% imported fiber
Initial pressure drop350 PaAt 1 m/min filtration velocity, clean tube
Operating pressure drop<1,500 PaGlass industry duty typically 900–1,300 Pa at 1 m/min
Breakage rate<0.2% within 3 yearsWith correct installation; tubes virtually never snap in service
Service life (incl. fittings)>5 yearsCounted from 168-hour acceptance
Production capacity72,000 tubes / year
Lead time<60 days

Material and performance envelope across the range:

PropertyValue
ChemistryAl₂O₃ + SiO₂ >90%
ColorWhite / cream
Density360–420 kg/m³
Temperature grades600 °C continuous-service grade; peaks up to 1,000 °C; maximum operating temperature 1,050 °C
Pore size range10–180 μm, graded through the wall
Compressive strength>1,000 N
Impact resistance>0.6 MPa
Max filtration velocity1.5 m/min
Typical particulate emission<1 mg/Nm³
Static resistance350 Pa
Max element size3,000 mm long × Ø150 mm, 1.4 m² filtration area per element
CapturesPM2.5 and sub-micron particles

Sizes and Selection: 36 Standard Models

Ceramic filter tube sizes and flange types
Ceramic filter tubes in different sizes and flange types

Standard elements cover lengths from 500 to 3,000 mm, outer diameters of 60 / 120 / 150 mm and inner diameters of 40 / 80 / 110 / 120 mm, with T-type or Y-type flanges. Filtration area runs from 0.2 to 1.4 m² per element and unit weight from about 0.4 to 9.5 kg.

Two build series are available: white non-catalyst tubes (AW series) and catalyst-loaded DeNOx tubes (AC series), both in ultra-high-temperature and end-reinforced builds.

Model (example)Length mmOD / ID mmFlangeArea m²Weight kg
AW50050060 / 40T0.20.4
AW10001,000150 / 110T0.483.2
AW12501,25060 / 40T0.230.8
AW20002,000150 / 110T1.05.0
AW30003,000150 / 110T1.48.5
AW19501,950150 / 110Y1.05.0
AW24002,400120 / 80T0.95.5

Full model list and selection logic: → Ceramic Filter Element Selection Guide

Catalyst-Loaded Tubes: DeNOx Verified by the CAS Process Institute

Catalyst-loaded ceramic filter tubes for DeNOx
Catalyst-loaded ceramic filter tubes for DeNOx duty

Catalyst performance was tested by the State Key Laboratory of Multiphase Complex Systems, Institute of Process Engineering, Chinese Academy of Sciences, on Ø60 × 50 mm (10 mm wall) catalyst tube samples. Test conditions: face velocity 0.5–0.8 Nm/min (working-face velocity 0.9–1.8 m/min), inlet NO 700 ppm (1,400 mg/Nm³), ammonia-to-NOx molar ratio 1, 170–450 °C, with 300 ppm SO₂ (900 mg/Nm³) and 10 vol.% H₂O in the sulfur/water cases.

Mid-temperature catalyst tube: in sulfur- and water-free gas, DeNOx approaches the theoretical rate from 240 °C. With 900 mg/Nm³ SO₂ and 10% water vapor present, low-temperature activity drops, but above 280 °C water and SO₂ have little effect. Recommended operation at 280 °C or above; below 280 °C, keep SO₂ under 35 mg/Nm³ for long-cycle running.

Low-temperature catalyst tube: in sulfur- and water-free gas it reaches 90% DeNOx at 180 °C and approaches the theoretical rate from 200 °C. With SO₂ and H₂O present it still holds 80% at 180 °C and exceeds 90% at 200 °C. Recommended operation at 180 °C or above to avoid water condensation; for long service life keep SO₂ within 5–30 mg/Nm³.

Both tubes are applicable to glass furnaces, biomass power, waste incineration, hazardous waste and coking flue gas. → Low-Temperature DeNOx: How Catalytic Ceramic Filters Work at 170–300 °C · → Catalytic Ceramic Fiber Filter product page

Strength, Service Life and Verification

A third-party test to GB/T 3002-2017 (refractories — hot modulus of rupture) measured a hot bending strength of 1,016.14 N at 600 °C. Combined with the >1,000 N compressive rating, this is why breakage stays below 0.2% over three years when installation rules are followed — and why filter life is counted in years, not bag-change cycles. Catalyst-loaded tubes carry a 7–9 year catalyst service life with 5 years guaranteed.

Non-catalyst version: → Non-catalyst Ceramic Fiber Filter

Where Hot Gas Filtration Is Already Working

Ceramic filter tubes installed inside a hot gas dust collector
Ceramic filter tubes installed inside a hot gas dust collector
  • Ultra-high-temperature filtration: fumed silica and alumina production, converter off-gas, metal smelting, chemical processes
  • SCR DeNOx: glass furnaces, biomass and wood-waste firing, waste-to-energy plants
  • Acid gas–solid separation and acid recovery: hydrochloric and sulfuric acid duty
  • Combustible gas cleaning: municipal waste and biomass biogas
  • Heavy and precious metal recovery: uranium, nickel, cobalt, lithium, gold, silver, palladium, platinum and their oxide residues

Documented installations include glass furnaces in Spain and Costa Rica, medical waste incinerators and metal melting furnaces. → Applications · → Dioxin Removal from Waste Incinerator Flue Gas

Commissioning and Operation Essentials

Ceramic tubes run differently from bags in one respect: commissioning matters. The documented procedure:

  1. Binder burn-out — heat the gas through the elements slowly to 160 °C and hold 160–170 °C for 16 hours to decompose the organic binder safely.
  2. Pre-coating — dose preconditioning powder (300–400 mesh hydrated lime Ca(OH)₂, talc, SiO₂, Al₂O₃ or class-1 fly ash) to build a 200 g/m² protective layer; about 40 g per 1,000 mm element or 300 g per 3,000 mm element, repeated for at least three full cleaning cycles.
  3. Pulse cleaning — never pulse at or below the dew point; use dry, oil-free compressed air at 0.35–0.55 MPa (200 ms pulse duration, 20–60 min interval, ΔP-triggered), clean between upper and lower ΔP limits and avoid over-cleaning, which is as harmful as under-cleaning. Stable ΔP is normally reached within 24–48 hours.
  4. Monitoring — watch the outlet with a triboelectric probe or opacity meter; anything above 5 mg/Nm³ (or above the usual level) signals a leak to trace back to its module. Fluorescent powder (5–10 g/m² filter area) with UV light inspection on the clean-gas side pinpoints any seal leaks before hot start-up.
  5. Shutdowns — keep the unit above 120 °C during shutdown to prevent condensation, seal inlet and outlet against moisture, and repeat the full commissioning procedure after long stops.

→ Pre-coating Ceramic Filter Tubes: Why It Matters and How to Do It · → Installation and Fluorescent Leak Detection Step by Step

What to Send with Your RFQ

To size a unit or quote replacement elements, send: gas flow (Nm³/h), operating and peak temperature, dust loading and dust chemistry, acid gas / NOx / dioxin concentrations and emission targets, available footprint and tubesheet layout (for retrofits), and compressed air availability. Element drawings, flange type (T/Y) and quantity speed up replacement quotes.

Request a Quote

Frequently Asked Questions About Hot Gas Filtration

Hot gas filtration cleans industrial exhaust at high temperature — in this system up to 1,050 °C — using rigid ceramic fiber filter tubes instead of fabric bags. Dust is captured on the tube surface and removed by pulse-jet cleaning, and with sorbent injection and catalyst-loaded tubes the same vessel also removes acid gases, NOx and dioxins.
The catalog rating is 600 °C continuous, peaks up to 1,000 °C, and a maximum operating temperature of 1,050 °C. This covers glass furnaces, incinerators, kilns and metal smelting duty without pre-cooling the gas.
Particulate outlet stays below 1 mg/Nm³. Integrated trains with dry sorbent and catalyst achieve SO₂ ≤30 mg/Nm³, NOx ≤50 mg/Nm³ (S.T.P., dry), DeNOx efficiency above 95% at 280 °C and up to 99.5% dioxin destruction (TEQ) by selective catalytic oxidation.
A clean 3,000 mm tube starts at about 350 Pa at 1 m/min filtration velocity. Operating differential pressure stays below 1,500 Pa; glass industry duty typically runs at 900–1,300 Pa.
Service life including fittings exceeds 5 years, counted from the 168-hour acceptance test, with a breakage rate below 0.2% in the first three years under correct installation. Catalyst in catalyst-loaded tubes lasts 7–9 years with 5 years guaranteed.
Yes. The tubes mount on the same tubesheet and pulse-jet cleaning concept as filter bags, so a baghouse can be converted by changing elements and internals. See the retrofit checklist.
Yes. Commissioning includes a binder burn-out at 160–170 °C for 16 hours, then pre-coating with about 200 g/m² of conditioning powder — roughly 40 g per 1,000 mm element — repeated over at least three cleaning cycles.
Standard lead time is under 60 days, with an annual production capacity of 72,000 tubes.