Guangzhou, Guangdong , China.

allan.lun@anchorgd.com

+86 13703050828

Non-catalyst Ceramic Fiber Filter

Non-catalyst hot gas filter

Non-catalyst Ceramic Fiber Filter Product Description Non-catalyst Ceramic Fiber Filter  is a porous filter for dedusting, which is made of refractory fiber and binder according to a certain scientific ratio. Its maximum long-term use temperature is up to 1100℃, so that the dedusting system doesn’t need to cool down, and can recover the heat energy […]