Non-catalyst Ceramic Fiber Filter
Non-catalyst Ceramic Fiber Filter is a porous filter for dedusting, which is made of refractory fiber and binder according to a certain scientific ratio.
Its maximum long-term use temperature is up to 1100℃, so that the dedusting system doesn’t need to cool down, and can recover the heat energy directly.
In dedusting, its use method and pulse backflush cleaning method are basically the same as that of the bag filter. But its service life is up to 10 years, which is several times longer than that of the bag filter, and it can resist acid and alkali corrosion.
Product model and size specifications
Code | Model | AW1500 | AW320 | AW3000 |
A | Length(mm) | 1500 | 300 | 3000 |
B | Internal diameter(mm) | 40 | 110 | 110 |
C | External diameter(mm) | 60 | 150 | 150 |
D | Flange diameter(mm) | 80 | 190 | 190 |
E | Flange thickness(mm) | 20 | 30 | 30 |
F | Surface areas(m2) | 0.28 | 0.1 | 1.34 |
G | Weight(kg) | 1.2 | 1.5 | 11.8 |
Remark: It is normal for the actual size of the product to differ slightly from the above table.
Please contact technical support for specific tolerance range.
Illustration: Below is Ceramic fiber filter’s dimension diagram :
Application:
Thermal power plants, waste incinerators, cement kilns, metallurgical industries, brick plants, biomass boilers and other dust generated scenes
Work efficiency:
Dust residual after dedusting<5mg/Nm3
Dedusting efficiency>99.9%
Remark: The removal rate of the pollutants in the flue gas depends on the performance of the additives, as well as the design, construction, and the operation level of the equipment.
Catalytic Ceramic Fiber Filter
Added the catalyst on the basis of the white filter can get catalytic ceramic fiber filter, which is a porous filter integrated multi-functions of dedusting, desulfurization, denitrification, de-acid gas, and de-dioxin.
Its desulfurization and denitrification efficiency are up to 95%, far exceeding the national standards. And it can remove the dioxin directly.
Use it for denitrification and de-dioxin can not only greatly reduce the supporting equipment and the overall area of the whole system, but also the various kinds of supporting operation costs.
Product model and size specifications
Code | Model | AC1500 | AC320 | AC3000 |
A | Length(mm) | 1500 | 300 | 3000 |
B | Internal diameter(mm) | 40 | 110 | 110 |
C | External diameter(mm) | 60 | 150 | 150 |
D | Flange diameter(mm) | 80 | 190 | 190 |
E | Flange thickness(mm) | 20 | 30 | 30 |
F | Surface areas(m2) | 0.28 | 0.1 | 1.34 |
G | Weight(kg) | 1.35 | 1.6 | 12.8 |
Remark: It is normal for the actual size of the product to differ slightly from the above table.
Please contact technical support for specific tolerance range.
Illustration: Below is Ceramic fiber filter’s dimension diagram :
Application:
Glass furnaces, steel furnace, biomass boiler, thermal power plant, waste incinerator, coking plant, metallurgical smelting furnace, etc.
Work efficiency:
NOx<50mg/Nm3 SO2<35mg/Nm3 | Up to 97% HCL removal Up to 95% SOx removal Up to 95% NOx removal Up to 97% dioxin removal |
Remark: The removal rate of the pollutants in the flue gas depends on the performance of the additives, as well as the design, construction, and the operation level of the equipment.